Recyclable retort packaging made of polypropylene is considered an important alternative to classic PET/aluminium/PP laminates. But switching to mono-materials alone is not enough. A decisive component often remains overlooked: the laminating adhesive. New developments show that even demanding sterilization applications can now be realized using solvent-free adhesive systems.
When people talk about recyclable flexible packaging, they usually discuss films. About mono-PE and mono-PP, barrier layers, EVOH content, and how to meet the requirements of the European Packaging and Packaging Waste Regulation (PPWR).
In doing so, a component essential to the function of a multi-layer packaging is easily overlooked: the laminating adhesive.
Especially in the case of sterilizable stand-up pouches, its task is demanding. It must permanently bond different film layers together, withstand high temperatures and moisture, and retain its properties even after months in contact with the packaged contents.
At the same time, it must not impair the recyclability of the entire structure.
The interesting insight: Of all things, switching to solvent-free adhesives could solve several of these challenges simultaneously.
1. Recyclability is not decided by the film alone
Conventional retort pouches often consist of a combination of PET, aluminium foil, and CPP. These laminates offer high barrier properties and are established for thermally demanding applications.
From the perspective of mechanical recycling, however, they are problematic. Combining different materials makes high-quality recovery difficult.
A possible alternative is structures consisting predominantly of polypropylene. For example:
- A three-layer laminate made of OPP, high-barrier OPP, and CPP.
- A two-layer laminate made of OPP and a coextruded CPP structure with EVOH barrier.
However, even if the films used are fundamentally compatible with recycling, the question regarding the remaining components remains.
In the Design-for-Recycling criteria for flexible PP packaging presented at INNO-Pouch 2026, the adhesive share also plays a role.
For PU laminating adhesives, the presented criteria specify a limit value of 5 % by weight of the total structure for the most favorable evaluation category.
This sounds like a generous limit at first. However, for thin film structures with multiple adhesive layers, it can certainly become relevant.
Three-layer laminates in particular require two lamination steps. If a comparatively high adhesive coat weight is used on both sides, the amounts add up.
Thus, adhesive technology itself becomes an integral part of design for recycling in packaging.
An important distinction must be made here: A low adhesive content alone does not guarantee recyclability. The actual compatibility of the adhesive with the recycling process and all other components of the packaging must also be taken into account.
2. Solvent-free lamination offers multiple benefits at once
In the flexible packaging industry, a shift towards solvent-free laminating adhesives has been emerging for years.
In a market evaluation presented at INNO-Pouch, their share of adhesive consumption rose from 25 to 38 percent between 2020 and 2024.
There are several reasons for this.
In solvent-based lamination, the solvent must be removed after application via a drying tunnel. This process consumes energy and requires appropriate equipment and exhaust air technology.
With solvent-free systems, this step is eliminated.
The comparative values presented in the lecture highlight the potential:
| Metric | Solvent-based | Solvent-free |
|---|---|---|
| Typical adhesive coat weight | 3.0–5.0 g/m² | 1.6–2.2 g/m² |
| Drying tunnel | Required | Not required |
| Energy consumption during lamination | Reference | Up to 65 % lower |
| CO₂ emissions from lamination | Reference | Up to 60 % lower |
The potential savings are derived from comparative data presented by MORCHEM. They are not automatically transferable to every plant and production process.
Nevertheless, the connection is remarkable: A lower adhesive coat weight not only reduces material consumption, but also facilitates compliance with Design-for-Recycling limit values.
In addition, there is an economic aspect. Less energy, lower application quantities, and eliminating solvent drying can reduce process costs.
This makes the development interesting not only from a sustainability perspective.
The same technology that can enable more recyclable packaging also offers potential for more economical production.
3. Why retort packaging has traditionally posed a special challenge
If solvent-free adhesives offer such advantages, why haven’t they been used for all flexible packaging for ages?
The answer lies primarily in the varying performance requirements.
Retort packaging is typically sterilized at temperatures around 121 °C. Heat, moisture, and pressure act on the entire packaging structure during this process.
At the same time, certain packaged goods can place high chemical stress on the laminate.
Wet pet food or other aggressive contents, for example, are particularly critical.
The adhesive layer must not detach under these conditions. Blistering, delamination, or visual defects are also unacceptable.
Classic solvent-based adhesives have a technological advantage here: they can be based on higher molecular weight polymers whose viscosity is lowered by the solvent for processing.
Solvent-free systems lack this option.
They must already possess a sufficiently low viscosity at processing temperature. This limits formulation options and makes it more difficult to simultaneously achieve very high chemical and thermal resistance.
The central development task is therefore:
How can the performance of a highly resistant solvent-based laminating adhesive be combined with the processing advantages of a solvent-free system?
4. New adhesive systems achieve the required bond strength
That this challenge can be solved was demonstrated by Federica Arioli, R&D Director at Spanish adhesive manufacturer MORCHEM, at INNO-Pouch 2026 in Barcelona.
In her presentation “Laminating adhesives: the hidden enabler of mono-material pouches”, she presented results of a two-component, solvent-free aliphatic polyurethane adhesive.
The evaluated system MORCHEM PL 292 A + CF 892 was specifically developed for demanding retort applications and aggressive packaged goods.
The results on a three-layer PP structure composed of OPP, high-barrier OPP, and CPP are particularly interesting.
The laminates were filled with wet pet food and subsequently sterilized under the following conditions:
- Sterilization at 121 °C for 30 minutes.
- Testing of bond strength before and after sterilization.
- Comparison with an established solvent-based reference system.
- Additional storage testing at 40 °C.
According to the manufacturer, the measured bond strengths exceeded 4 N/15 mm. This applied to both adhesive interfaces of the three-layer laminate.
According to Arioli, corresponding bond strengths were also achieved with printed structures.
No visible defects such as blistering or delamination occurred during the testing.
Particularly remarkable: In individual measurements, the solvent-free system even achieved higher bond strengths than the solvent-based reference product.
The results demonstrate that solvent-free adhesives, when suitably formulated, can also be considered for thermally and chemically demanding packaging applications.
However, these are results from a specific adhesive system under defined test conditions. General transferability to all film combinations and contents cannot be inferred from this.
5. The actual challenge begins after sterilization
Packaging that possesses high bond strength immediately after sterilization is not automatically suitable for a long shelf life.
Especially with moist and chemically demanding products, the bond between the film layers must remain stable over the entire shelf life.
For this reason, the investigated laminates were additionally stored at 40 °C after sterilization.
According to the presented results, the solvent-free system demonstrated stable bond strength over a period of six months. Here too, it achieved comparable or in some cases better values than the reference system.
This is an important step.
For the practical suitability of a retort package, it is not only decisive whether it survives the sterilization process. It must also reliably fulfill its protective function during storage and transport.
Alongside mechanical stability, food safety plays a central role in this context.
With polyurethane adhesives, particular attention must be paid to the potential formation or migration of primary aromatic amines (PAAs).
The adhesive system presented is based on aliphatic polyurethane chemistry. MORCHEM reports no PAA migration for the system and points to compliance with the requirements of Regulation (EU) No 10/2011.
For specific applications, testing of the finished packaging under the intended conditions of use remains necessary.
6. From laboratory development to real-world packaging
Technically interesting laboratory results are one thing. What matters, however, is whether an industrially viable package can be developed from them.
A particularly practical example was presented during the lecture.
Together with customers, MORCHEM realized a two-layer PP retort structure containing an EVOH barrier within a CPP structure.
The structure consists of a printed outer OPP film, an adhesive layer, and a coextruded CPP structure with EVOH.
The advantage over a three-layer structure: only one adhesive layer is required.
The following properties were specified for the example presented:
- Adhesive content below 3 % by weight.
- EVOH content of maximum 5 % by weight.
- Sterilizability.
- Solvent-free lamination.
- Stated shelf life of more than twelve months.
The example demonstrates that a PP-based barrier retort packaging can be realized with a comparatively low amount of adhesive.
The data on shelf life and recyclability refer to the presented application and should not be taken as general proof for all comparable structures.
Nevertheless, the result is relevant: the development is not limited to a theoretical material combination, but has already been transferred into a concrete packaging solution.
7. A limit value alone is not sufficient for recycling assessment
An interesting discussion arose after the presentation regarding the question of different assessment systems for recyclability.
While the presented European design-for-recycling criteria specify a limit of 5 % by weight for PU laminating adhesives, according to the speaker, RecyClass operates with stricter requirements of 3 %.
This highlights a problem for packaging developers.
A structure may meet the requirements of a specific assessment system, while another system arrives at a different classification.
In addition, limit values for individual components represent only part of the recycling assessment.
The actual processing in the recycling process must also be taken into account.
For packaging developers, this means that the choice of adhesive should not be made solely on the basis of coat weight.
Equally relevant are its chemical composition, interactions with the remaining materials, and behavior in the intended recycling process.
The development of suitable testing methods and the harmonization of assessment criteria therefore remain important tasks.
8. What the results mean for the development of flexible packaging
Several conclusions for packaging development can be drawn from the investigations presented.
First: Mono-material is a system task.
It is not enough to replace PET with PP or swap an aluminum barrier for EVOH. Films, printing inks, barrier layers, and adhesives must be considered holistically.
Second: Less material can also make economic sense.
Lower adhesive coat weights, the elimination of solvent drying, and simpler laminate structures can help reduce both the environmental footprint and manufacturing costs.
Third: The boundaries of solvent-free lamination are shifting.
Applications long considered the domain of solvent-based adhesives are increasingly being opened up to solvent-free systems. The results presented on sterilized PP laminates show the potential that exists here.
Fourth: Testing must go beyond the sterilization process.
Bond strength immediately after thermal treatment is only part of the requirements. Long-term stability, chemical resistance, food safety, and barrier function must be evaluated together.
Conclusion: The invisible component becomes a key development factor
The discussion on recyclable retort packaging often focuses on selecting suitable film materials. In doing so, it is easy to overlook how heavily the properties of a package depend on its thinnest functional layers.
Current developments in solvent-free laminating adhesives show that significant potential lies here.
Lower coat weights make it easier to meet design-for-recycling requirements. Dispensing with solvents can reduce energy demand and emissions. At the same time, new formulations enable bond strengths that withstand even demanding sterilization conditions.
This overcomes another technical hurdle on the path to recyclable retort pouches.
However, this does not mean that every existing retort package can already be converted seamlessly to mono-PP. Barrier requirements, packaged goods, processing conditions, and recycling infrastructure remain crucial.
The key takeaway is therefore not that a new adhesive solves all problems, but that the development of recyclable high-performance packaging only succeeds when supposedly invisible components are factored in right from the start.
And perhaps that is precisely where an economic opportunity lies: if material use, energy consumption, and complexity can be reduced without compromising the protective function of the packaging, design-for-recycling solutions can become not only regulatorily necessary, but also attractive from a manufacturing perspective.
This article is based on the presentation and lecture “Laminating adhesives: the hidden enabler of mono-material pouches” by Federica Arioli, R&D Director at MORCHEM, at INNO-Pouch on October 8/9, 2026 in Barcelona. The testing and performance data shown originate from the investigations presented by MORCHEM. Further information: www.morchem.com.